Solution of fully enclosed process of water-based

2022-07-22
  • Detail

"Water-based wood paint" for wood furniture, wood floors, wooden houses, wood fences and other wood products, just like putting a layer of protective clothing on these wood products, it can not only skillfully cover the defects of the wood surface, but also better highlight the original texture of the wood, and protect the wood from damage. Due to the low characteristic solid content and film-forming material content of water-based wood paint, the film hardness of water-based paint is not high. Therefore, it is a difficult problem for water-based wood paint to achieve the effect of full sealing compared with the water-based paint industry

as a "burdink water-based paint" that has been deeply studied in the water-based wood paint industry for 15 years, with the joint efforts of burdink people, it has successfully broken through the problem of "full sealing effect of water-based paint". Next, I'll share with you the solution of the full sealing process of waterborne wood paint:

at present, the full sealing process of waterborne wood paint can be divided into three types: the full sealing process of "water under oil", "the full sealing process of waterborne paint grinding filler", and the full sealing process of "waterborne primer and finish". The oil bottom and water surface technology and water-based paint polishing and filling technology are mainly suitable for big mane materials, such as oak, Manchurian ash, etc; The fully enclosed process of water-based primer and finish is suitable for small mane materials, such as pine, maple, cherry, etc

I. Introduction to the full sealing process of oil bottom and water surface:

1: white embryo grinding

2: rubbing the bottom and color

3: two to three times of water-based special Pu primer (depending on the size of the wood bristle eye)

4: water-based color trimming

5: water-based topcoat

precautions: the oil bottom and water surface technology is operable and practical, but the oil primer should be fully dry to ensure that there is no residual odor

II. Introduction to the full sealing process of water-based paint (small bristle eye material):

1: white embryo grinding

2: water-based cementitious primer (function: sealing wood, burring)

3: grinding

4: water-based Riess

5: water-based primer two to three times (the number of primer spraying times depends on the size of wood bristle eye, until the desired paint film effect is achieved)

6: water-based color trimming

7: water-based topcoat

precautions: the waiting time for each coat of primer to dry shall be sufficient, and each coat of primer must be polished in place to avoid collapse. Because the water-based primer is sprayed too many times, the polishing must be in place to ensure the film thickness and not affect the transparency

III. introduction to the full sealing process of water-based paint grinding filler:

1: white embryo grinding

2: water-based cementitious primer (function: sealing wood, burring)

3: grinding filler, water-based color paste, evenly wipe or scrape, and after it is completely dry, polish the surface of wood tendon to dry, leaving only bristle eye color

4: water character Rees

5: two to three times of water-based primer, depending on the size of the wood brown eye

6: water-based color trimming

7: water-based topcoat

precautions: the grinding filler must be wiped or scraped into the bristle hole to avoid pits. The surface must be polished clean, otherwise it will affect the adhesion of the primer

from the above three processes, the oil bottom water surface full sealing process is the simplest, the grinding filler full sealing process is slightly complex, and the pure water-based full sealing process requires too much material